Two different coatings undergo the same test. A world of difference after ISO 12944-9 CX testing. How do we do this at M2LAB?

Not all coatings are equal

Difference in corrosion result after ISO 12944-9 CX test
The panels in the photo have both undergone 4,200 hours of cyclic corrosion testing according to ISO 12944-9 CX. Each panel had a different coating. A scribe was made in the paint beforehand to measure the corrosion that developed from it during the test. Despite both being properly blasted and having the same coating thickness, the difference in results is enormous.
The test according to ISO 12944-9 CX is used to determine whether a coating is suitable for use in extremely corrosive conditions, such as offshore. But how exactly does certification according to ISO 12944-9 work?

How we carry out the ISO 12944-9 CX test at M2LAB

Step 1: The paint system is applied to blasted steel panels measuring 150 × 75 mm and at least 3 mm thick. Step 2: The test panels are stored for two weeks under standard laboratory conditions. Step 3: A scribe 2 mm wide is applied to the panels, cutting through the paint and any zinc layer. Step 4: The coating thickness and adhesion are measured.
Offshore test conditions ISO 12944-9 CX
Step 5: The test panels are exposed to a cyclic load consisting of:
  • 3 days alternating 4 hours UV light and 4 hours water condensation
  • 3 days salt spray test
  • 1 day freezing cold at -20 °C
This cycle is repeated for 25 weeks. Step 6: The loosened paint around the pre-applied scribe is removed. The extent of corrosion that has developed around the scribe is then measured. In addition, an assessment is made of overall rusting, blistering, cracking and flaking. Step 7: After 7 days of conditioning at 23 °C and 50% relative humidity, the adhesion of the coating is measured again and assessed against the evaluation criteria.

Evaluation criteria ISO 12944-9 CX

  • Blistering (ISO 4628-2): 0
  • Rusting (ISO 4628-3): Ri0
  • Cracking (ISO 4628-4): 0 (S0)
  • Flaking (ISO 4628-5): 0 (S0)
  • Corrosion from scribe ≤ 3 mm (≤ 8 mm for high impact areas)
  • Adhesion (ISO 4624): minimum adhesion strength of 5 MPa per measurement. 0% failure between steel and first layer, unless the minimum adhesion strength of 5 MPa is achieved.
The coating is approved when at least 2 of the 3 tested panels meet all of the above requirements.

De Coating Nerd

“Waar ik ook ben, op mijn werk of als ik vrij ben, ik kijk naar alles waar een verflaagje op zit. Helemaal als er iets mis mee is. Roestplekken, blaasjes en afbladderende verf, daar word ik gelukkig van! Nou ja, gelukkig… dat is wat overdreven. Maar ik vind het machtig interessant. Wat een mazzel heb ik dan ook dat ik hier mijn beroep van heb mogen maken. De hele dag onderzoek doen aan verfsystemen, ge(poeder)coate voorwerpen en bedrijven helpen bij het verbeteren van hun product.”

Latest articles

Any questions?

Have a question? Want to consult with an expert about which test is best for you? Would you like to have a test performed? If so, please contact us.

Questions? Get in touch with one of our specialists!